We have a project the will run Zytel PA66 101L, the customer is asking to boil the parts at 80c for 8 hours. Has anyone had experience doing this? I know that nylon will stop absorbing moisture once it comes to equilibrium. My pass experience was to just package the parts in a box lined with a plastic bag, add water and zip tie the bag shut. Years ago I remember a nylon part the we put in hot water, but I cannot remember the length of time...