17th August 2018, 05:04 PM
#1
Re: Flaring
Does it flare as soon as it ejects or even before? We had a part similar that bowed inwards and we dropped it straight in water and found it kept its shape better. The part was made out of peek though at high temperatures.
-
18th August 2018, 05:00 AM
#2
Re: Flaring
I'm wondering, is it possible that the flaring caused by material itself? I mean that's a fake resin perhaps...