    I agree with Jendalf, could be a problem with the surface temperature in the mould. Also check that you have a melt cushion during injection holding phase or that the holding pressure time is not too...
  2. Replies
    5
    Views
    4,893

    Re: Nitrogen Sealing

    I have run this material before. In my situation we fitted a plate with a feed throat orifice underneath the hopper slider. The plate had a small hole drilled horizontally in it from the outside into...
  3. Replies
    4
    Views
    5,929

    Re: Barrel jackets

    One thing to consider, if there is a possibility of running heat sensitive materials in the future e.g.POM, I would recommend having a removeable jacket section at the front of the barrel over the...
  4. Replies
    6
    Views
    7,539

    Re: Foaming agents

    This is the advice I used to give to technicians who were having issues with foaming agents, based on my own experience:

    INJECTION MOLDING WITH FOAMING AGENTS