Search:

Type: Posts; User: stevenchengcn; Keyword(s):

Search: Search took 0.00 seconds.

  1. Re: “Splay” issue on PA66 GF30% with UV stabiliser.

    My experience: PA+GF,the barrel and nozzle temperature from the material supplier is 280 degree.the surface is awful,while the temperature decrease t0 235-240 degree,all is ok.
    also many times,my...
  2. Replies
    7
    Views
    10,195

    Re: Sticking Sprue

    I couldn't agree any more,the same problem occured here,too long and thin sprue,some circle undercut on inner surface.
    shorten the sprue bush(lathe a hole on the cavity side) and change a good...
  3. Replies
    6
    Views
    7,354

    Re: hot runner

    Hi Pilot,
    As far as I know,most hoturnner system components are standard,very few is customised.
  4. Re: Polycarbonate

    Hi
    It happened that I have a website for the PC injection molding treatment:http://www.myplasticmold.com/injection-moulded-product.html
  5. Re: Gate Seal Time / Holding Time for Hot Runners

    No,I didn't heard that
  6. free calculator for the injection cooling system

    Hi ,I have build a calculator for the calculation of the cooling time of injection molding,it is totally free:http://www.myplasticmold.com/cooling-time-calculation-of-injection-molding.html
  7. Replies
    5
    Views
    5,780

    Re: Need Help... Injection or Mold issue?

    Yes,Ruhlj,But I think water basin shouldn't be small one,and my question is :when did you find this problem?form the begining of manufacturing or after a period of time?
  8. Replies
    2
    Views
    6,295

    Re: hot runner molds

    Yes,there are other brand for the hotrunner system,like yudo from korea,ZDQ from china.We normally use the heat coil "hotset " from Germany.