Don't care if its mold, mold design, tolerances, material, or if its just the customer. ( You know the one that wants the part in plastic with properties of steel, or tell you set the mach on...
Type: Posts; User: ATI K ID; Keyword(s):
Don't care if its mold, mold design, tolerances, material, or if its just the customer. ( You know the one that wants the part in plastic with properties of steel, or tell you set the mach on...
No pictures but should of. I was out of town acquiring two more pieces of equipment and on the day I got back I was walking by press with an armload of bar stock and just dropped all of it. The...
PA 6/6 has good heat and chemical resistance. I make electric terminal connections with that.
I had a guy completley encase a barrel on a 500T in a very stiff PC all the way to the feedthroat, yeah good times.........................
Stuff peeled right off.
Easiest screw/barrel clean was with asaclean EX grade pulled a screw out of a 500T with less than 50lbs. force and screw took less than 5 min. to clean I mean NO DEPOSITS left.
DME J-series and don't get over 25% rg it will be not to your advantage aesthetically
Asaclean EX grade works way better that the styrene and it cuts screw cleaning time to nothing.
I've encountered this before check all connections and re-seat boards in panel and op station. I have the same machine.