Hi,
when the tool was at maintenance, it might be also the grease coming out of the insert nearby the gate. Or ejectors, but thats not the case according to the picture.
Disasembly the tool again...
This year I´ve forgotten to wish you out and in. Obviously reasonable.
But I´m glad that this community lives and resurrect the post despite that.
It was a hard year for everybody, I wish you...
Hello,
have somebody tried to use standard IM Machine for injecting of the silicone?
Lets assume 1-component silicone, curing by temperature.
Material filling thru standard feeding throat at...
Input card reading the position from transducer.
this will not work as the nikom writes.
overmold ABS than TPE on it is not a right way.
but generally how you want to do that? inject XXX thousends buttons than change material and insert it into...
yes
it depends on the % of content.
you can make some improovements by process and setup, like tool temperature for better filler orientation.
try 5-10 % and test for cracking. This content is...
Can you setup the automatic lubrication? there will be setting which you can solve your problem.
If its not working properly than contact technical support at F-M, They will know for sure what to...
Hi,
the issue is in the material used.
Try to think about some filler - like glass fiber for example.
There is no need to make any other correction in the tool or process.
Let us know.
J.
And what was the problem?
Hello,
I can recommend the book where are all this rules are well described.
Injection Molding Advanced Troubleshooting Guide (eBook)
The 4M Approach
Author: Kerkstra, R., Brammer, S.
exactly...this is first think to check.
Than memory modul itself - Exchange.
J.
Oh man you don´t want to....otherwise you would have to pay the price for gallon also for liter :D
:) but the number is not normal :)
Hi,
can you post here the process output datas and injection curve with time and preassure scale?
J.
Hi,
I´m not at the machine, and will not be for some time.
Try to found it there, you have to choose what you want to export, which sheets or pictures.
thats what the picture actually says :)...
Hi, its there-...try to look for
444445
J.
Hi,
yes, its problem. Change the design or material (silicon would work).
J.
Hello,
interesting topic.
I would go the way of holding or fixing the strips into the cavity too.
Inserts like Nemanja has, can be one way. The other is tool design with core positioning like...
Hi,
check this for NA:
http://fimmtech.com/
this for GER:
https://www.spritzguss-schulung.de/
For ENG/GER:
https://kunststoff-institut-luedenscheid.de/
here is the contact on the support. I have only on Nissei europe.
Mr. Jhonny Depoorter
j.depoorter@nissei.be
Technical service
if You want a phone, write me and PM here.
than I have...
Heat up!
Heads up,
Work hard,
Mold part!
Greetings and hello all again...
Jan
Merry Christmass and Happy New Year to all good people here.
Machines has finally stopped, alle hot runners went cold, all gates has frozen :)
Backup Your data and switch off the pumps!
Enjoy...
Hi,
the "issue" is the difference of the temperatures used for each type of polymer.
1)
Establish the procedure of cleaning every time You have to change from Higher melt polymer (PC, PA,...
Hi,
You have to have also special fittings and connectors.
Tool have to be prepared for this as higher water temperature than boiling temp. means higher preassure to keep the water "liquid".
...